Browning

Browning

84-May 24 2022 06_41am-7Rfj

Soil test.

20220701_095818

Soiled area

close-up of carpet browning and soil wicking showing discoloration at fiber tips after drying

Browning

84-May 24 2022 06_41am-7Rfj 20220701_095818 close-up of carpet browning and soil wicking showing discoloration at fiber tips after drying

Browning / Soil Wicking (Carpet)

Floor Detective® Claims and Conditions Guide

Summary

Browning and soil wicking are post-wetting discoloration conditions that develop as carpet dries following cleaning or water exposure. Discoloration appears primarily at the tips of the face yarns due to moisture-driven migration and concentration of materials within the carpet system. The condition does not represent fiber wear, dye instability, or inherent manufacturing failure and is often evaluated alongside related conditions. See also Soiling, Appearance Retention, and Carpet Problems for broader context.

Please subscribe to see all content

Carpet Problems

Carpet problems may involve seams, backing systems, texture changes, traffic wear, mechanical damage, or installation-related conditions.
Read More
Carpet Problems

Carpet Fiber Identification (Field and Laboratory Methods)

Carpet fiber identification helps determine how carpet may respond to heat, moisture, cleaning chemistry, abrasion, and environmental exposure.
Read More
Carpet Fiber Identification (Field and Laboratory Methods)

Wool and Wool Carpet Properties

Wool carpet properties include moisture absorption, chemical sensitivity, shedding, and appearance variation associated with natural wool fibers.
Read More
Wool and Wool Carpet Properties

Carpet Beetle Damage

Carpet beetle damage is localized fiber loss caused by larvae feeding on organic materials within carpet, often occurring in concealed...
Read More
Carpet Beetle Damage

Fiber Properties

Carpet fiber properties determine durability, resilience, and how flooring performs under traffic and environmental conditions.
Read More
Fiber Properties

Missing Row

Carpet missing rows are manufacturing-origin tufting conditions involving absent yarn along machine-direction rows.
Read More
Missing Row

Browning

Browning and soil wicking are discoloration conditions caused by moisture-driven migration of materials to the carpet surface during drying.
Read More
Browning

Wrinkles in Backing

Carpet backing wrinkles are manufacturing-related distortions caused by backing misalignment, tension variation, or latex lock-in.
Read More
Wrinkles in Backing

Unraveling / Runs (Carpet)

Carpet unraveling runs are progressive yarn withdrawals that follow tuft rows in continuous filament carpet constructions.
Read More
Unraveling / Runs (Carpet)

Core Crush / Roll-Core Pile Reversal (Carpet)

Carpet roll-core crush occurs when pile yarns become compressed around the roll core, creating visible light or dark banding near...
Read More
Core Crush / Roll-Core Pile Reversal (Carpet)